Designation:A626/A626M−16StandardSpecificationforTinMillProducts,ElectrolyticTinPlate,DoubleReduced1ThisstandardisissuedunderthefixeddesignationA626/A626M;thenumberimmediatelyfollowingthedesignationindicatestheyearoforiginaladoptionor,inthecaseofrevision,theyearoflastrevision.Anumberinparenthesesindicatestheyearoflastreapproval.Asuperscriptepsilon(´)indicatesaneditorialchangesincethelastrevisionorreapproval.ThisstandardhasbeenapprovedforusebyagenciesoftheU.S.DepartmentofDefense.1.Scope*1.1Thisspecificationcoversdouble-reducedelectrolytictinplateproducedfromlow-carboncold-reducedsteelfurnishedincoilsandcutsizesforusepredominatelyinthemanufactureofcans.Itisfurnishedincommerciallyavailabletincoatingweights[masses]andisnormallysuppliedwithatrimmededge.1.2Thisspecificationisapplicabletoordersineitherinch-poundunits(asA626)whichissuppliedinthicknessesfrom0.0050to0.0118in.orSIunits[asA626M]whichissuppliedinthicknessesfrom0.127to0.300mm.1.3Thevaluesstatedineitherinch-poundorSIunitsaretoberegardedasstandard.Withinthetext,theSIunitsareshowninbrackets.Thevaluesstatedineachsystemarenotexactequivalents.Therefore,eachsystemmustbeusedindepen-dentlyoftheother.Combiningvaluesfromthetwosystemsmayresultinnonconformancewiththisspecification.1.4Thisstandarddoesnotpurporttoaddressallofthesafetyconcerns,ifany,associatedwithitsuse.Itistheresponsibilityoftheuserofthisstandardtoestablishappro-priatesafetyandhealthpracticesanddeterminetheapplica-bilityofregulatorylimitationspriortouse.2.ReferencedDocuments2.1ASTMStandards:2A623SpecificationforTinMillProducts,GeneralRequire-mentsA623MSpecificationforTinMillProducts,GeneralRe-quirements[Metric]A630TestMethodsforDeterminationofTinCoatingWeightsforElectrolyticTinPlateA754/A754MTestMethodforCoatingWeight(Mass)ofMetallicCoatingsonSteelbyX-RayFluorescenceB339SpecificationforPigTin3.OrderingInformation3.1Ordersforproductunderthisspecificationshallincludethefollowinginformation,asrequiredandapplicable,todescribeadequatelythedesiredproduct:3.1.1Na...